Platcheta et al. (2013) Fig. 6. Results of XRR and their analysis: model for fitting procedure (x-axis not shown up to scale), where ρ is the density and d is the sample thickness (a), experimental XRR curve and fitting results for a sample deposited at 25 % of O2/(O2 + Ar) with thickness of 100 nm (b), XRR curves for thicker samples (Table 1) deposited at 5–15 % (c) and 15–30 % (d) of O2/(O2 + Ar) flow ratio.

Image 341667 is a 2694 by 2756 pixel WebP
Uploaded: Apr6 24


Last Modified: 2024-04-06 17:43:02
Permanent URL: https://serc.carleton.edu/download/images/341667/ti_oxide_xrr_results_1-s2.0-s0169433222025740-gr6_lrg.webp

The file is referred to in 1 page
Provenance
Figure from Płacheta, K., Kot, A., Banas-Gac, J., Zając, M., Sikora, M., Radecka, M. and Zakrzewska, K., 2023. Evolution of surface properties of titanium oxide thin films. Applied Surface Science, 608, p.155046. Used under Creative Commons License.
Reuse
This item is offered under a Creative Commons Attribution-NonCommercial-ShareAlike license http://creativecommons.org/licenses/by-nc-sa/3.0/ You may reuse this item for non-commercial purposes as long as you provide attribution and offer any derivative works under a similar license.